Grade 202
Standard Cr-Mn austenitic grade — the workhorse 200-series stainless.
Material Overview
Cr-Mn Austenitic
AISI 202 is one of the most widely produced and consumed stainless steel grades in the world. With ~17% chromium and 4-6% nickel balanced by manganese and nitrogen, it offers a strong combination of strength, formability, and corrosion resistance at a competitive price.
Equivalent / Comparable: AISI 202 / EN 1.4373
Indicative Price
₹165 – ₹195 / kg
Available Forms
Coils
Sheets
Plates
Slit Coils
Circles
Chemical Composition
Typical wt% Range
| Element | Range (wt%) |
|---|---|
| C | ≤0.15 |
| Mn | 7.5–10.0 |
| Si | ≤1.0 |
| P | ≤0.06 |
| S | ≤0.03 |
| Cr | 17.0–19.0 |
| Ni | 4.0–6.0 |
| N | ≤0.25 |
Mechanical Properties
Density7.80 g/cm³
Tensile Strength≥ 655 MPa
Yield Strength≥ 310 MPa
Elongation≥ 40%
Hardness (HRB)≤ 95
Key Utility & Strengths
- ▸Higher strength than 304 due to nitrogen
- ▸Good formability and weldability
- ▸Adequate atmospheric corrosion resistance
- ▸Excellent for indoor architectural use
Industries Served
Where Grade 202 is Used
ArchitectureAutomotiveKitchenwareRailway CoachesPublic Infrastructure
Typical Applications
End-Use Components
Railings, gates, balustrades
Automotive wheel covers & trim
Bus body & coach interiors
Kitchen equipment & appliances
ATM enclosures, signage
Why Choose 202 from Nivesha Alloys
- ✓Globally recognised AISI specification
- ✓Lower cost vs. 304 with comparable strength
- ✓Excellent availability across forms
As an authorised Jindal Stainless co-branding channel partner, all material is supplied with Mill Test Certificates ensuring full traceability and compliance.